754
Co-based superalloys

GH605

Product Size

Φ5-300mm、sheet/plate

Applicable Specifications

National Standard (GB),Enterprise Standard


Key Properties

Good stress-rupture and creep properties, excellent oxidation resistance and weldability


Application Fields

Aerospace, Nuclear Power

Learn More Products