Corrosion-Resistant Alloys

N08800

Product Size

Ф60-550mm

Applicable Specifications

ASTM/AISI, National Standard (GB), Enterprise Standard

Key Properties

Excellent high-temperature resistance, good general corrosion resistance

Application Fields

Chemical, Petroleum, Nuclear Power, Energy, Environmental Protection