728
Fe-based superalloys

GH2132(A286\660)

Product Size

Φ6-400mm、forgings, cylinders, wire

Applicable Specifications

National Standard (GB), Enterprise Standard

Key Properties

Good tensile strength, yield strength, and elongation below 650°C, with good oxidation and corrosion resistance; grain size difference ≤2 grades

Application Fields

Aviation, Aerospace, Steam Turbines, etc.