Product Size
Φ20-300mm
Enterprise Standard
High strength, low expansion coefficient, good thermal fatigue resistance, and nearly constant elastic modulus below 650°C; grain size difference ≤2 grades; stable batch performance, PPK >1.33
Aviation, Aerospace