727
Fe-based superalloys

GH2674

Product Size

Φ10-700mm

Applicable Specifications

National Standard (GB), Enterprise Standard

Key Properties

Good tensile strength, yield strength, and elongation below 650°C, with good oxidation and corrosion resistance

Application Fields

Steam Turbines

Learn More Products