Forged bar
>Ф90mm-Ф400mm
Rolled bar
Ф8mm-Ф90mm
Cold-drawn ba
Ф3.5mm-Ф65mm
Enterprise Standard, Agreements
This low-alloy ultra-high strength steel has tensile strength ≥1600 MPa, good strength-toughness balance, and good processability and weldability.
Aerospace