Ultra-High-Strength Alloys

D6AC

Forged bar

>Ф90mm-Ф450mm

Rolled bar

Ф8mm-Ф90mm

Cold-drawn ba

Ф3.5mm-Ф65mm

Applicable Specifications

ZHSD/JT-17-0044

Key Properties

D6AC is improved from 4340 steel, offering excellent low-temperature toughness and fracture toughness.

Application Fields

Aerospace

Learn More Products