Ultra-High-Strength Alloys

9310(9310)

Forged bar

>Ф90mm-Ф450mm

Rolled bar

Ф8mm-Ф90mm

Cold-drawn ba

Ф3.5mm-Ф65mm

Applicable Specifications

AMS 6265

Key Properties

Ni-Cr-Mo alloy carburizing steel; high surface hardness after carburizing, good core toughness; tensile strength ~1000–1200 MPa; excellent wear and impact resistance.

Application Fields

Aerospace