Bar
Φ7-350mm
Slab
(75–180 thickness) × (450–800 width) × 1200 mm
ASTM/AISI, National Standard (GB), Enterprise Standard
Sufficient high-temperature strength at 700–750°C, good oxidation resistance below 900°C; service temperature ≤750°C (long-term), up to 900°C short-term
Aerospace, Energy Industry, Additive Manufacturing