Ni-based superalloys

GH4220

Product Size

Φ16-22mm

Applicable Specifications

National Standard (GB),Enterprise Standard

Key Properties

Stable performance at 900–950°C; suitable for hot-section components such as blades

Application Fields

Aviation, Aerospace, etc.