About Shangda
Superalloys & High-Performance Alloys
High-Quality Special Stainless Steels
Qualification Certificates
Technical Support & Service Assurance
Product Size
Φ45-52.5mm
National Standard (GB), Enterprise Standard
Excellent high-temperature strength below 850°C; used for gas turbine blades
Aviation, Aerospace, etc.