Ni-based superalloys

GH4037

Product Size

Φ10-150mm

Applicable Specifications

ASTM/AISI, National Standard (GB), Enterprise Standard

Key Properties

For higher temperatures, GH4037 is strengthened by Al, Ti, plus solid solution strengthening with Mo and W, and grain boundary strengthening with B and Ce; maintains high thermal strength at 850°C. Good microstructural stability and high oxidation resistance during long-term service at 850°C

Application Fields

Aerospace

Learn More Products