About Shangda
Superalloys & High-Performance Alloys
High-Quality Special Stainless Steels
Qualification Certificates
Technical Support & Service Assurance
Product Size
Φ8.5mm-460mm
National Standard (GB), Enterprise Standard
Good oxidation and corrosion resistance, high stress-rupture strength
Aviation, Aerospace, Others