Ni-based superalloys

GH4080A(Nimonic80A)

产品规格

Φ5.5-300mm

Applicable Specifications

ASTM/AISI, National Standard (GB), Enterprise Standard

Key Properties

Good creep resistance in the range 650–850°C; short-term service up to 850°C, maximum service temperature about 800–815°C. Density ~8.15 g/cm³, non-magnetic. Good cold and hot workability, and capability for automatic argon arc welding and seam welding

Application Fields

Aerospace, Steam Turbines, Energy, Nuclear Power, Petrochemical/Oil gas

Learn More Products